Fast setting repairing mortar R3
POTENTIAL CAUSES OF THE PROBLEM
a) Application of fi nal coat plaster directly on AAC blocks.
b) Application was not made with the proper tools
SOLUTION
STEP 1: Clean thoroughly with a brush, the surface from dust loose particles
STEP 2: Start repairing the cracked surface with the fast setting, repairing mortar WRM 520 (R3)
STEP 3: Prime the surface with deep penetration primer, GLX 292 FLEX PRIM
STEP 4: Apply the fi rst layer of fi ber-reinforced, base coat, THC 410
STEP 5: As long as THC 410 is still wet, firmly CLIMAPLUS fi berglass mesh (160 g/m2)
STEP 6: Then, apply a second layer of fi ber-reinforced, base coat, THC 410, in order to completely cover the mesh
STEP 7: Prime the surface of application with the colored acrylic primer GLX 494 PRIM
STEP 8: Apply the organic acrylic based top coating DEC 428, at the color tone of our selection from CLIMAPLUS fan deck
ATTENTION: In case that the application is at a seaside area or area with high moisture content, THRAKON suggests the application of our silicone system. In such case, proceed to the following steps:
STEP 7: Prime the surface with the colored silicone based primer GLX 498 SIL PRIM
STEP 8: Application of organic silicone based top coating DEC 438, at the color tone of our selection from CLIMAPLUS fan deck