After application of the paint, there are scars from brush or roller

POTENTIAL CAUSES OF THE PROBLEM

a) The work was done with shoddy tools (brushes, rollers, etc.)

b) The application of many layers (more than the rest of the surface) at the same point (brush or roller)

c) Application of poor quality paint

SOLUTION

1: Rubbing and good cleaning of the surface with a brush

2: Fill where required with STATUS 100% acrylic stucco

3: Prime with primer STATUS POLYPRIMER

4: Apply two layers of  STATUS ECO

Products used: