Fix exterior paint blistering/bubbling

POTENTIAL CAUSES OF THE PROBLEM

Problem insufficient adhesion, resulting from:

a) Probably rained shortly after the paint was applied

b) Possible moisture from the substrate

c) Apply paint with prohibitive weather conditions (high temperatures)

SOLUTION

1: With a sandpaper remove all loose and then wipe the surface thoroughly

2: Fill where required with STATUS 100 % acrylic putty

3: Prime with Primer STATUS DUR SOLVENT

4: Apply STATUS ALL WEATHER in two layers

Products used: